Product
Hydrophilic modifier
HS45M
Dispersant(emulsifing thickener)
Dispersant(emulsifing thickener)series scope
     HWP10Z      HWP80Z
     HWP25Z      HWP40F
     HWP60Z      HWP55F
     HWP70Z      HWP50F
     HWP30Z  
Modified polyvinylalcohol
Instant polyvinyl alcohol
Sizing agent for paper
Leather sizing series
Cotton fabric mortar
Electronic screen photosensitive resist
 Plastic membrane
Redispersible emulsion powder
Well cementing fluid loss additive
 
online
 
 
 
 
HWP70Z

Product standard:

Item

Index

HWP70Z

Appearance

White powder

Viscositympa•s

36.0-42.0

Saponification degree%(mol/mol)

78.5-81.5

PH value

5.0-7.0

Fugitive constituent %

≤5.0

Ash content%

≤0.5

Using method:
1, Weight: dosage is up to polymerization formulation and solution concentration
2, Put the normal temperature miring water in the dissolving tank, and stir it.
3, Put it into dissolving tank slowly in case of caking.
4, Stirring it to make it fully swelling. (Notice: If put it into hot water (>50°C), it is easy to form cakes.)
5, Heat it gradually and make the temperature to 70-80°C in 30 minutes (Notice: do not heat it quickly and the temperature should not be so high. If the temperature is higher than 80°C, it will appear precipitate.), and then keep stirring for 60 minutes.
6, Cooling: Cool the solution to below 30°C, and put the transparent solution after filtration into storage tank, then get some of it to analyze its solid content. (Notice: when it is stored in hot summer, the solution is easy to turn white when the temperature is higher than 40°C. So, it is feasible to set the pipe coil to below 25-30°C to guarantee the polymerization process.)

 